Viva VS
HIGHLY TRANSLUCENT ZIRCONE
MULTI LAYER & PROGRESSIVE FLEXURAL STRENGTH
Transparency is gradual from 44% to 47%. The flexural strength is also progressive from 800 to 1100 MPa. VS zirconia suitable for any type of indication, it is ideal for single frames and long-span bridges.

Flexural strength | 800 à 1100 MPa |
Thermal expansion (25-500°C) | (10.5 ± 0.5) ×10-6·K-1 |
Composition | ZrO2 + HfO2, Y2O3,Fe2O3, Al2O3, Er2O3,… |
Translucency | 44 % a 47% |
Sintering temperature | 1480°C for 2 hours |